List Of Welding Flux
| Metals |
Thickness, mm |
TIG (AC) |
TIG (Ar, He, Ar+He, etc.) (DC) |
LASER CO2 |
MIG |
| FRONT |
BACK |
FRONT |
BACK |
FRONT |
BACK |
FRONT |
BACK |
| Aluminium Alloys |
< 4,0 (1 pass) |
|
Scouring & Forming Flux |
Activating & Scouring Flux |
Scouring & Forming Flux |
|
Scouring & Forming Flux |
|
Scouring & Forming Flux |
| >4,0 (1,2,3, etc.) |
Activating & Scouring Flux |
Scouring & Forming Flux and Flux Tape |
Activating & Scouring Flux |
Scouring & Forming Flux and Flux Tape |
Activating & Scouring Flux |
Scouring & Forming Flux |
Activating & Scouring Flux |
Scouring & Forming Flux and Flux Tape |
| Magnesium Alloys |
0,8-4,0 (1 pass) |
|
Scouring & Forming Flux and Flux Tape |
|
Scouring & Forming Flux and Flux Tape |
|
Scouring & Forming Flux |
|
Scouring & Forming Flux and Flux Tape |
| Carbon Steels |
<10 (1 pass) |
|
|
Activating Flux |
|
|
|
|
|
| >10 (2,3, etc. passes) |
|
|
Activating Flux
(1 pass) |
|
|
|
|
|
| Stainless Steels |
<10 (1 pass) |
|
|
Activating Flux |
Protecting & Forming Flux |
Activating Flux* |
Scouring & Forming Flux |
|
Protecting & Forming Flux* |
| >10 (2,3,
etc. passes) |
|
|
Activating Flux (1 pass) |
Protecting & Forming Flux |
Activating Flux* |
Scouring & Forming Flux |
Activating Flux |
Protecting & Forming Flux* |
| Titanium Alloys |
<10 (1 pass) |
|
|
Activating Flux |
|
Activating Flux* |
|
|
|
| >10 (2,3, etc. passes) |
|
|
Activating Flux (1 pass) |
|
Activating Flux* |
|
|
|
| Nickel Base Alloys |
<10 (1 pass) |
|
|
Activating Flux |
|
Activating Flux* |
|
|
|
| >10 (2,3, etc. passes) |
|
|
Activating Flux (1 pass)* |
|
Activating Flux (1 pass)* |
|
|
|
| Zirconium Base Alloys |
<10 (1 pass) |
|
|
Activating Flux |
|
Activating flux* |
|
|
|
| >10 (2,3, etc. passes) |
|
|
Activating Flux (1 pass)* |
|
Activating flux* |
|
|
|
Notes: * - Researches are carried out
|